Troubleshooting a welding system is imperative for detecting welding defects and reducing the chances of a reduced quality product. There are a variety of ways to check for welding defects in your system such as checking for shielding gas leaks and flow and spatter, replacing welding tips and liners regularly, checking welding wire, and checking the stick out height or push pull angles. For more information on checking welding defects, contact Robots.com experts today.

Welding automation robots with ferris wheel positioner


Robot Weldingdefects are something that manufacturers want to try to avoid at all costs. When a robotic welder produces defects during the welding process, it can cut down on the integrity of the weld, which can take away from the quality of the product. That is why it is important to understand how to troubleshoot your robotic system if you see welding defects.

Porosity is one of the most common welding defects. It can be caused by a shielding gas leak or a clogged welding gun nozzle. This can cause welds to be made from undercut or cold roll material, causing defects in the weld. There are many different steps you can run through to check for porosity issues and other welding defects in yourrobotic weldingsystem.

5Steps to Checking Porosity Issues in Your Fanuc Welding Robot

  1. Check for Shielding Gas Leaks and Flow– When checking for a shielding gas leak, use soap bubbles, and make sure all fittings are tight. The shielding gas flow should feel like it is coming out of the gun, but not enough to cause any turbulence or disruption.
  2. Check for Spatter– A welding nozzle can get bogged down with spatter over time. Remove the weld nozzles from the robot system, inspect them, and clean any weld spatter before replacing them.
  3. 定期替换焊接技巧和衬垫– Welding contact tips should be replaced daily to ensure that the wire feed is smooth and consistent during each welding cycle. Welding liners need to be replaced weekly in shops that run three shifts per day.
  4. Check Welding Wire– The welding wire should feel strong as it exits the welding gun. To preventbird nests”, a tangle of wire that halts the wire from being fed, flip the drive roll and pull the wire back out of the gun. Then trim the tangled wire and re-thread it through the feeder and back to the gun.
  5. Check Stick Out Height and Push Pull Angles– The typical stick out height for a welding robot, the distance from the end of the welding gun nozzle and tip to the weld joint, is58inches to34inches. Ensure that the measurement is correct, and check all the push pull angles of the system. Steel usually requires a drag angle of around15degrees, while aluminum requires a15degree lead angle to burn of oxides with the arc.

Once you have completed all of these steps, you should be able to correct theweldingdefects, like porosity, and return to a strong, durable welding application that will be high quality and consistent.